Worm Tracks

Worm Tracks are often encountered in both self-shielded and gas shielded flux core arc welding (FCAW). They are caused by gas that has come out of the solidifying weld but has been trapped under the slag. Worm Tracks are also called: Elongated Porosity (AWS A3.0 2010) Gas marks Chicken Feet Chicken Tracks Elongated Porosity is […]

Worm Tracks Read More »

Image of Tungsten Electrodes

Tungstens – Don’t Just Pick A Colour

In manufacturing, TIG welding, also known as Gas Tungsten Arc Welding (GTAW), is known for its precision and high-quality welds. TIG welding produces clean, precise welds with minimal spatter, making it ideal for applications requiring aesthetically pleasing welds of exceptional quality. TIG welding is suitable, among other things, for:    Stainless steels Aluminium and nickel

Tungstens – Don’t Just Pick A Colour Read More »

Circumstances in which arc rectification occurs

Arc Rectification

When Gas Tungsten Arc Welding (GTAW) oxide-forming materials such as aluminium and magnesium, DCEN for penetration and DCEP for its cleaning action can be used together. This is referred to as Alternating Current (AC) welding. Figure 1 (a). Representation of a sinusoidal voltage Figure 1 (b). Representation of a square wave voltage In both the

Arc Rectification Read More »